I-ASTM A572 steel angle enye i-high-strength, low-alloy (HSLA) izigaba zensimbi ze-columbium-vanadium. Ngenxa yenani elincane lezinto ze-columbium & vanadium alloy, i-engeli yensimbi eshisayo engu-A572 inezakhiwo ezingcono kune-carbon steel A36. Okokuqala, i-A572 inamandla aphezulu kune-A36 njengamandla esivuno namandla aqinile. Okwesibili, kulula ukushisela, ukwakha kanye nomshini.
I-angle yensimbi enamandla angu-A572
Ama-engeli ensimbi anama-galvanized & Pre-lacquered
I-angle yensimbi ye-A572 inezinhlelo zokusebenza ezibanzi ngenxa yesilinganiso esiphakeme samandla nesisindo. Ngenxa yokuthi ayinakho okuqukethwe kwethusi okuwusizo ekumelaneni nokubola, ama-engeli ensimbi yesakhiwo A572 ngokuvamile aba ama-hot-dip galvanized noma pre-lacquered. Umbala womdwebo usesicelweni sakho.
Incazelo ye-engeli yensimbi ye-A572:
Qaphela: Osayizi bensimbi ye-engeli ekhethekile bayatholakala uma inani le-oda lakho lidlula inani elincane.
Izici ze-engeli yensimbi ye-A572 nezinzuzo:
Into | Ibanga | Ikhabhoni, ubuningi, % | I-Manganese, ubuningi, % | I-silicon, ubuningi, % | Phosphorus, ubuningi, % | Isibabule, ubuningi, % |
I-Engeli yensimbi ye-A572 | 42 | 0.21 | 1.35 | 0.40 | 0.04 | 0.05 |
50 | 0.23 | 1.35 | 0.40 | 0.04 | 0.05 | |
55 | 0.25 | 1.35 | 0.40 | 0.04 | 0.05 |
Into | Ibanga | Yield Point, min, ksi [MPa] | Amandla Okuqina, min, ksi [MPa] |
I-Engeli yensimbi ye-A572 | 42 | 42 [290] | 60 [415] |
50 | 50 [345] | 65 [450] | |
55 | 55 [380] | 70 [485] |