KỌMICAL TI 30CRMOV9
| C |
Mn |
Si |
P |
S |
Kr |
Ni |
Mo |
V |
| 0.26-0.34 |
0.40-0.70 |
0.40 ti o pọju |
ti o pọju 0.035 |
ti o pọju 0.035 |
2.30-2.70 |
0.60 ti o pọju |
0.15-0.25 |
0.10-0.20 |
Awọn ohun-ini ẹrọ ti 30CRMOV9
| Ilana |
Iwọn (mm) |
Agbara Fifẹ Rm (Mpa) |
Agbara Ikore Rp0.2 (Mpa) |
Ilọsiwaju A5 (%) |
Ipa Iye Kv (J) Iwọn otutu yara |
| KÚNCHED O SI RU |
160 o pọju |
900 iṣẹju |
700 iṣẹju |
12 min |
35 min |
| KÚNCHED O SI RU |
160-330 |
800 iṣẹju |
590 min |
14 min |
35 min |
Awọn ohun-ini ARA TI 30CRMOV9
| module odo (GPa) |
Ipin Poisson (-) |
Modulu rirẹ (GPa) |
Ìwọ̀n (kg/m3) |
| 210 |
0.3 |
80 |
7800 |
| Apapọ CTE 20-300°C (µm/m°K) |
Agbara ooru kan pato 50/100°C (J/kg°K) |
Imudara igbona iwọn otutu ibaramu (W/m°K) |
Atako eletiriki otutu ibaramu (µΩm) |
| 12 |
460 - 480 |
40 - 45 |
0.20 - 0.25 |
Itọju gbigbona TI 30CRMOV9:
- Annealing rirọ: ooru si 680-720oC, dara laiyara. Eyi yoo ṣe agbejade lile lile Brinell ti o pọju ti 248.
- Nitriding:
- Gaasi / pilasima nitriding otutu (gaasi, iwẹ iyọ): 570-580oC
- Gaasi / pilasima nitriding otutu (lulú, pilasima): 580oC
- Dada líle lẹhin nitriding: 800 HV
- Lile: Lile lati iwọn otutu ti 850-880oC ti o tẹle pẹlu pipa epo.
TEMPERING TI 30CRMOV9:
IDAGBASOKE TI 30CRMOV9:
- Gbona lara otutu: 1050-850oC.
Awọn apẹrẹ ti o wa:
- Pẹpẹ dudu / Pẹpẹ Alapin / Ọpa onigun /Pipe, /Steel strip, /sheet
- Imọlẹ – bó + didan, lilọ aarin
- Eda - oruka, tube, casing pipe, disiki, ọpa
Awọn ohun elo Aṣoju ti 30CRMOV9:
Awọn irin igbekale alloy ni a lo ni lilo pupọ ni ẹsun ti ọkọ oju omi, ọkọ, ọkọ ofurufu, misaili itọsọna, awọn ohun ija, ọkọ oju-irin, awọn afara, ohun elo titẹ, awọn irinṣẹ ẹrọ, awọn paati ẹrọ pẹlu iwọn apakan nla ati bẹbẹ lọ., Awọn jia ẹrọ, ọpa jia, akọkọ axis, ọpá àtọwọdá, Awọn ẹya ẹrọ - ọpa asopọ, boluti ati nut, Ọpa Multidiameter, Ohun elo titẹ, paipu ti ko ni oju