Önümler
We have professional sales team numbered 200 with more than 16 years experience.
Positionerleşişi:
Öý > Önümler > Polat plastinka > Boý güýji pes erginli polat
Q500F polat plastinka
Q500F polat plastinka
Q500F polat plastinka
Q500F polat plastinka

Q500F polat plastinka

Q500F polat plastinka köprüleriň gurluşygynda, awtoulag ýollarynyň gurluşygynda we beýleki in Engineeringenerçilik gurluşyklarynda ulanylýar
Himiki düzümi
STEEL GRADE C% iň ýokary Si% max Mn% max P% max S% max Cu% max Cr% max Ni% max Mo% max B% iň ýokary V% iň ýokary Nb% max Ti% max
Q500F 0.2 0.80 1.7 0.02 0.010 0.5 1.5 2 0.70 0.005 0.12 0.06 0.05
Mehaniki eýeçilik
STEEL GRADE Gaýtadan öndürijilik güýji Mpa min Gaýtadan öndürijilik güýji Mpa min uzalma% Energiýa we temperatura
Min 0 -20 -40 -60
  t≤50 50-100 100-150 t≤50 50-100 100-150   J. J. J. J.
Q500F 500 480 440 590-770 590-770 540-720 17 47 47 34 34
Degişli önümler
Sorag
* Ady
* E-poçta
Telefon
Countryurt
Habar