Komposisi Kimia sareng Sipat Mékanis:
ASTM A537 Kelas 3 (A537CL3)
BAHAN |
C |
Bungbulang |
Si |
P≤ |
S≤ |
ASTM A537 Kelas 3 (A537CL3) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
BAHAN |
Kakuatan Tensile (MPa) |
Kakuatan ngahasilkeun (MPa) MIN |
% Elongation MIN |
ASTM A537 Kelas 3 (A537CL3) |
485-690 |
275-380 |
20 |
ASTM A537 Kelas 2 (A537CL2)
BAHAN |
C |
Bungbulang |
Si |
P≤ |
S≤ |
ASTM A537 Kelas 2 (A537CL2) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
BAHAN |
Kakuatan Tensile (MPa) |
Kakuatan ngahasilkeun (MPa) MIN |
% Elongation MIN |
ASTM A537 Kelas 2 (A537CL2) |
485-690 |
315-415 |
20 |
ASTM A537 Kelas 1 (A537CL1)
BAHAN |
C |
Bungbulang |
Si |
P≤ |
S≤ |
ASTM A537 Kelas 1 (A537CL1) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
BAHAN |
Kakuatan Tensile (MPa) |
Kakuatan ngahasilkeun (MPa) MIN |
% Elongation MIN |
ASTM A537 Kelas 1 (A537CL1) |
450-585 |
310 |
18 |
Dokumén anu dirujuk
Standar ASTM:
A20/A20M: Spésifikasi pikeun Sarat Umum pikeun Tekanan Kapal Pelat
A435/A435: Pikeun Ujian Ultrasonik Lempeng-Beam tina Plat Baja
A577/A577M: Pikeun Ultrasonic Angle-Beam Ujian Pelat Baja
A578/A578M: Pikeun Ujian Ultrasonik Beam Lempeng tina Pelat Baja Gulung pikeun Aplikasi Husus
Catetan Manufaktur:
Lempeng baja handapeun ASTM A537 Kelas 1, 2 jeung 3 bakal ditelasan baja tur sasuai jeung sarat ukuran sisikian austenitic rupa Spésifikasi A20 / A20M.
Métode perlakuan panas:
Sadaya pelat dina ASTM A537 kedah dirawat panas sapertos kieu:
Pelat ASTM A537 Kelas 1 kedah dinormalisasi.
Kelas 2 jeung Kelas 3 piring kudu quenched jeung tempered. Suhu tempering pikeun pelat Kelas 2 teu kudu kurang ti 1100°F [595°C] jeung teu kurang ti 1150°F [620°C] pikeun pelat Kelas 3.