Stainless Steel 347/ 347H BUSHING
Stainless Steel 347/ 347H TEE
Beurat % (sadaya nilai maksimum iwal rentang disebutkeun béda)
unsur | 347 | 347H |
Kromium | 17.00 mnt.-19.00 max. | 17.00 mnt.-19.00 max. |
Nikel | 9.00 mnt.-13.00 max. | 9.00 mnt.-13.00 max. |
Karbon | 0.08 | 0,04 mnt.-0,10 max. |
Mangan | 2.00 | 2.00 |
Fosfor | 0.045 | 0.045 |
Walirang | 0.03 | 0.03 |
Silikon | 0.75 | 0.75 |
Columbium & Tantalum | 10 x (C + N) min.-1,00 max. | 8 x (C + N) min.-1,00 max. |
Beusi | Kasaimbangan | Kasaimbangan |
SIFAT FISIK
Kapadetan: 0,288 lbs/in3 7,97 g/cm3 Résistansi Listrik: microhm-in (microhm-cm): 68 °F (20 °C): 28,7 (73)
Panas spésifik: BTU/lb/°F (kJ/kg•K):
32 - 212 °F (0 - 100 °C): 0,12 (0,50)
Konduktivitas Termal: BTU/hr/ft2/ft/°F (W/m•K):
Dina 212 °F (100 °C): 9.3 (16.0)
Dina 932 °F (500 °C): 12.8 (22.0)
Rata-rata Koéfisién Ékspansi Termal: in/in/°F (µm/m•K):
32 - 212 °F (0 - 100 °C): 9,3 x 10·6 (16,6)
32 - 1000 °F (0 - 538 °C): 10,5 x 10·6 (18,9)
32 - 1500 °F (0 - 873 °C): 11,4 x 10·6 (20,5)
Modulus élastisitas: ksi (MPa):
28 x 103 (193 x 103) dina tegangan
11 .2 x 103 (78 x 103) dina torsi
Perméabilitas magnét: H = 200 Oersteds: Annealed <1.02 max
Rentang Lebur: 2500 - 2550 °F (1371 - 1400 °C)