Stainless Steel 347/ 347H BUSHING
347H TEE 347H TEE
Weight % (litheko tsohle li holimo ntle le haeba ho boletsoe ka tsela e 'ngoe)
Element | 347 | 347H |
Chromium | 17.00 min.-19.00 max. | 17.00 min.-19.00 max. |
Nickel | 9.00 min.-13.00 max. | 9.00 min.-13.00 max. |
Khabone | 0.08 | 0.04 mets.-0.10 max. |
Manganese | 2.00 | 2.00 |
Phosphorus | 0.045 | 0.045 |
Sebabole | 0.03 | 0.03 |
Silicone | 0.75 | 0.75 |
Columbium le Tantalum | 10 x (C + N) min.-1.00 max. | 8 x (C + N) min.-1.00 max. |
Tšepe | Ho leka-lekanya | Ho leka-lekanya |
LITŠOANTŠISO TŠEBELE
Boima: 0.288 lbs/in3 7.97 g/cm3 Ho hanyetsa Motlakase: microhm-in (microhm-cm): 68 °F (20 °C): 28.7 (73)
Mocheso o khethehileng: BTU/lb/°F (kJ/kg•K):
32 - 212 °F (0 - 100 °C): 0.12 (0.50)
Thermal Conductivity: BTU/hr/ft2/ft/°F (W/m•K):
Ho 212 °F (100 °C): 9.3 (16.0)
Ho 932 °F (500 °C): 12.8 (22.0)
Kakaretso ea Coefficient ea Katoloso ea Thermal: ho/in/°F (µm/m•K):
32 - 212 °F (0 - 100 °C): 9.3 x 10·6 (16.6)
32 - 1000 °F (0 - 538 °C): 10.5 x 10·6 (18.9)
32 - 1500 °F (0 - 873 °C): 11.4 x 10·6 (20.5)
Modulus of Elasticity: ksi (MPa):
28 x 103 (193 x 103) ka tsitsipano
11 .2 x 103 (78 x 103) ka torsion
Magnetic Permeability: H = 200 Oersteds: Annealed <1.02 max
Melting Range: 2500 - 2550 °F (1371 - 1400 °C)