Kuumbwa Kwemakemikari%
Giredhi |
C |
Si |
P |
S |
Cr |
Mn |
Ni |
Fe |
310 |
0.025 max |
1.50 max |
0.045 max |
0.03 max |
24.0 - 26.0 |
2.0 max |
19.0-22.0 |
Remainder |
310S |
0.08 max |
1.50 max |
0.045 max |
0.03 max |
24.0 - 26.0 |
2.0 max |
19.0-22.0 |
Remainder |
Mechanical Properties
Kusimba Simba (ksi) |
0.2% Kusimba Kwegoho (ksi) |
Elongation% mu2 inches |
75 |
30 |
40 |
Zvinhu Zvenyama
|
310 |
310S |
Tembiricha mu°C |
Density |
8.0 g/cm³ |
9.01 g/cm³ |
Room |
Specific Heat |
0.12 Kcal/kg.C |
0.12 Kcal/kg.C |
22° |
Melting Range |
1400 - 1455 °C |
1399 - 1454 °C |
- |
Modulus yeElasticity |
193 - 200 KN/mm² |
200 KN/mm² |
22° |
Electrical Resistivity |
77 µΩ.cm |
94 µΩ.cm |
Room |
Coefficient of Kuwedzera |
15.8 µm/m °C |
14.4 µm/m °C |
20 - 100 ° |
Thermal Conductivity |
16.2 W/m -°K |
13.8 W/m -°K |
20° |
Fabrication DataAlloy 310 inogona kusungirirwa zviri nyore uye kugadziridzwa neyakajairwa chitoro chekugadzira maitiro.
Sravana Sameeralu Serial 4th Hot FormingKupisa zvakafanana pa 1742 - 2192 ° F (950 - 1200 ° C). Mushure mekupisa kugadzira anneal yekupedzisira pa1832 - 2101 ° F (1000 - 1150 ° C) inoteverwa nekudzima nekukurumidza kunokurudzirwa.
Cold KuumbaIyo alloy inonyatso ductile uye inoumba nenzira yakafanana zvikuru ne 316. Kutonhora kuumba zvidimbu nekugara kwenguva refu kune tembiricha yakakwirira hazvikurudzirwe sezvo alloy iri pasi pecarbide precipitation uye sigma phase precipitants.
WeldingAlloy 310 inogona kugadzirwa nyore nyore neakawanda akajairwa maitiro anosanganisira TIG, PLASMA, MIG, SMAW, SAW uye FCAW.
Masevhisi Edu
1.Zvigadzirwa zvakagadzirwa:Kana iwe une dhizaini yako , tinokwanisa kugadzira maererano wako
2.Uwandu Guarantee:Waya dhayamita,Mesh hole ,Dimension ne clips zvinozovimbiswa
mutengo
4.Odha:Hapana maodha mahombe uye maodha madiki , tinogamuchirwa kuisa maodha kwatiri
5.Design:Customers’ dhizaini inotenderwa