Q345E hot rolled steel sheet Chemical composition
Mechnical property for Q345E low alloy structural steel:
Thickness (mm) |
Q345E |
≤ 16 |
> 16 ≤ 35 |
> 35 ≤ 50 |
>50 |
Yield strength (≥Mpa) |
345 |
325 |
295 |
275 |
Tensile strength (Mpa) |
470-630 |
Chemical composition for Q345E low alloy structural steel (Heat Analysis Max%)
Main chemical elements composition of Q345E |
C |
Si |
Mn |
P |
S |
V |
Nb |
Ti |
Al (min.) |
0.18 |
0.55 |
1.00-1.60 |
0.025 |
0.025 |
0.02-0.15 |
0.015-0.060 |
0.02-0.20 |
0.015 |
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Cutting and welding as per end user’s demands
♦ More striction on some chemical elements contains
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Ultrasonic test under GB/T2970,JB4730,EN 10160,ASTM A435,A577,A578
FAQ
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.