E24W4 steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.
E24W4 steel is the Equivalent grades as S235J2W ( 1.8961 ) steel in EN 10025 - 5 : 2004 standard and WTSt 37-3 steel in SEW087 standard and also Fe360DK1 steel in UNI standard
The specifications:
Thickness: 3mm--150mm
Width: 30mm--4000mm
Length: 1000mm--12000mm
Standard: ASTM EN10025 JIS GB
E24W4 Steel Chemical Composition
C % | Mn % | Cr % | Si % | CEV % | S % |
Max 0.13 | 0.2-0.6 | 0.4-0.8 | Max 0.4 | Max 0.44 | Max 0.3 |
Cu % | P % | ||||
0.25-0.55 | Max 0.035 |
E24W4 Steel Mechanical Properties
Grade
|
Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
E24W4 | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
Thick mm | ≤16 | >16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤150 |
≤3 | >3 ≤100 | >100 ≤150 | -20 | 27 |
E24W4 | 235 | 225 | 215 | 215 | 215 | 195 | 360-510 | 360-510 | 350-500 |
The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.
If E24W4 mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.