Komposisi Kimia lan Sifat Mekanik:
A516 Grade 70 Komposisi Kimia |
sasmita |
Elemen Maks (%) |
C |
Si |
Mn |
P |
S |
A516 kelas 70 |
|
|
|
|
|
Ketebalan <12,5 mm |
0.27 |
0.13-0.45 |
0.79-1.30 |
0.035 |
0.035 |
Ketebalan 12,5-50 mm |
0.28 |
0.13-0.45 |
0.79-1.30 |
0.035 |
0.035 |
Ketebalan 50-100 mm |
0.30 |
0.13-0.45 |
0.79-1.30 |
0.035 |
0.035 |
Ketebalan 100-200 mm |
0.31 |
0.13-0.45 |
0.79-1.30 |
0.035 |
0.035 |
Ketebalan > 200 mm |
0.31 |
0.13-0.45 |
0.79-1.30 |
0.035 |
0.035 |
Setara Karbon: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
sasmita |
|
A516 Grade 70 Properti Mekanik |
kekandelan |
ngasilaken |
Tarik |
Elongation |
A516 kelas 70 |
mm |
Min Mpa |
Mpa |
Min % |
Perawatan panas:
Piring kanthi kekandelan 40 mm [1,5 in] utawa ing ngisor iki biasane diwenehake ing kondisi sing digulung. Yen perlu dinormalisasi utawa ngilangi stres kudu dilaporake sadurunge pesenan.
Plat sing luwih saka 40 mm [1,5 in] kekandelan kudu dinormalisasi.
Yen tes ketangguhan kedudukan dibutuhake ing piring 1,5 in [40 mm] lan miturut kekandelan iki, piring kasebut kudu dinormalisasi kajaba ditemtokake dening sing tuku.
Disetujui dening panuku, tingkat cooling luwih cepet tinimbang cooling ing udhara sing diijini kanggo nambah kateguhan, kasedhiya piring sing banjur tempered ing 1100 kanggo 1300℉ [595 kanggo 705 ℃].
Dokumen Referensi:
Standar ASTM:
A20/A20M: Keperluan umum piring baja kanggo wadhah tekanan lan tank
A435/A435M: Spesifikasi kanggo pemeriksaan ultrasonik balok lurus saka piring baja
A577/A577M: Kanggo pemeriksaan ultrasonik amba-beam saka piring baja
A578/A578M: Kanggo pemeriksaan UT balok lurus saka piring sing digulung kanggo aplikasi khusus