Standar ASTM A537 nuduhake piring prau tekanan, bahan ing baja silikon karbon-mangan sing diolah panas. Adhedhasar kekuwatan lan perawatan panas sing beda-beda, kisaran Kelas 1, 2 lan 3. Ketebalan maksimum miturut ASTM A537 Kelas 1 yaiku 100 mm [4 inci], lan 150 mm [6 inci] kanggo Kelas 2 lan kelas 3.
A537 CL2 Heat treated Boiler steel plate Keterangan:
Baja ASTM A537 Kelas 2 minangka bahan ngasilake lan kekuatan tarik sing luwih dhuwur sing digunakake kanggo nggawe kapal bertekanan lan dandang baja. Baja kasebut kalebu paduan karbon, mangan lan silikon lan diolah kanthi panas nggunakake metode quenched lan tempered sing menehi kekuatan residual.
Komposisi Kimia lan Sifat Mekanik:
A537 kelas 2. Komposisi Kimia
sasmita Elemen Maks (%)
C Mn P S Si Cu Ni Cr Mo
A537 Kelas 2 0.24 0.92-1.72 0.035 0.035 0.13-0.55 0.38 0.28 0.29 0.09

sasmita A537 kelas 2. Properti Mekanik
kekandelan ngasilaken Tarik Elongation
A537 Kelas 2 mm Min Mpa Mpa Min %
-65 415 550-690 22
65-100 380 515-655 20
100-150 315 485-620 -


Standar ASTM:

A20/A20M: Spesifikasi kanggo Keperluan Umum kanggo Plate Kapal Tekanan
A435/A435: Kanggo Pemeriksaan Ultrasonik Lurus-Beam Plat Baja
A577/A577M: Kanggo Ultrasonik Sudut-Beam Pemeriksaan Plat Baja
A578/A578M: ​​Kanggo Pemeriksaan Ultrasonik Lurus-Beam Plat Baja Gulung kanggo Aplikasi Khusus

Cathetan Manufaktur:

Piring baja miturut ASTM A537 Kelas 1, 2 lan 3 kudu dipateni baja lan tundhuk karo syarat ukuran gandum austenitik sing apik saka Spesifikasi A20/A20M.

Metode Perawatan Panas:

Kabeh piring miturut ASTM A537 kudu diolah kaya ing ngisor iki:
Piring ASTM A537 Kelas 1 kudu dinormalisasi.
Piring kelas 2 lan kelas 3 kudu dipateni lan digawe panas. Suhu tempering kanggo piring Kelas 2 ora kudu kurang saka 1100°F [595°C] lan ora kurang saka 1150°F [620°C] kanggo piring Kelas 3.
Produk sing gegandhengan
Pelat baja bejana tekanan A285 GR.C
Plat baja ASTM A285 Grade B
Plat baja Boiler ASTM A285 Grade A
ASME SA 387 KELAS 22 Kelas 1
ASME SA 387 KELAS 12 Kelas 2
ASME SA 387 KELAS 22 Kelas 2
ASME SA 387 KELAS 12 Kelas 1
SA387 GR.21 CL1 Pressure vessel steel plate
ASME SA387 GR.22 CL2 Boiler and Pressure Vessel Steel plate
ASME SA387 GR.22 CL1 Pressure Vessel Steel plate
SA387 GR.12 CL2 Pressure Vessel Steel plate
SA387 GR.12 CL1 Alloy Pressure Vessel plate baja
ASME SA387 GR.11 CL2 Pressure Vessel Steel plate
ASTM A537 cl3 Alloy Pressure Vessel Plat Baja
A537 CL1 Plat Baja Kapal Tekanan Normalisasi
ASTM A537 Kelas 1,2,3 Boiler and Pressure vessel steel plate
ASME SA 387 KELAS 11 Kelas 2
ASTM A537
ASME SA387 Kelas 11
ASME SA353 Ni-alloy steel plates
ASME SA553 Steel plate
06Ni9DR
DIN Standard 10CrMo910 Pressure Vessel Steel Plate
JIS G3103 SB480M Boiler Steel Plate
Nakoni, nyelidiki
* jeneng
* E-mail
Telpon
negara
Pesen