Ngwakọta kemịkalụ nke 30CRMOV9
C |
Mn |
Si |
P |
S |
Cr |
Ni |
Mo |
V |
0.26-0.34 |
0.40-0.70 |
0.40 kacha |
0.035 kacha |
0.035 kacha |
2.30-2.70 |
0.60 kacha |
0.15-0.25 |
0.10-0.20 |
Ngwongwo nke 30crmov9
Usoro |
Dayameta (mm) |
Ike Tensile Rm (Mpa) |
Ike Mpụta Rp0.2 (Mpa) |
Mgbatị A5 (%) |
Mmetụta Uru Kv (J) Okpomọkụ ụlọ |
KWURU NA ONWE |
160 max |
900 min |
700 min |
12 min |
35 min |
KWURU NA ONWE |
160-330 |
800 min |
590 min |
14 min |
35 min |
AKWỤKWỌ MMỤỌ ARỤ 30CRMOV9
Youngs modul (GPa) |
Oke Poisson (-) |
Modul shear (GPa) |
Njupụta (kg/m3) |
210 |
0.3 |
80 |
7800 |
Nkezi CTE 20-300°C (µm/m°K) |
Ikike okpomọkụ akọwapụtara 50/100°C (J/kg°K) |
Okpomọkụ ikuku (W/m°K) |
Igwe ọkụ eletriki okpomọkụ (µΩm) |
12 |
460-480 |
40-45 |
0.20 - 0.25 |
Ọgwụgwọ okpomọkụ nke 30CRMOV9:
- Mkpuchi dị nro: ọkụ ruo 680-720oC, dị jụụ nwayọ. Nke a ga-emepụta ike Brinell kacha nke 248.
- Nitriding:
- Gas /plasma nitriding okpomọkụ (gas, nnu bath): 570-580oC
- Gas/plasma nitriding okpomọkụ (ntụ ntụ, plasma): 580oC
- Ike elu mgbe nitriding gasịrị: 800 HV
- Ịgbasi ike: Kposie ike site na okpomọkụ nke 850-880oC na-esote mmanụ quenching.
Ọkụ nke 30CRMOV9:
- Ọnọdụ okpomọkụ: 570-680oC.
Ịmepụta 30CRMOV9:
- Ọnọdụ okpomọkụ na-ekpo ọkụ: 1050-850oC.
Ụdị dị:
- Ogwe ojii / Ogwe dị larịị / Square mmanya /Pipe, /Steel strip, / mpempe akwụkwọ
- Na-egbuke egbuke – peeled + na-egbu maramara, egweri na-enweghị etiti
- Ehierọ - mgbanaka, tube, ọkpọkọ ọkpọkọ, diski, aro
Ngwa ahụkarị nke 30CRMOV9:
Alloy structural steels na-ọtụtụ ebe na-gbara akwụkwọ nke ụgbọ mmiri, ụgbọ ala, ụgbọ elu, eduzi agha, ngwá agha, ụgbọ okporo ígwè, àkwà mmiri, nrụgide ụgbọ, igwe ngwá ọrụ, n'ibu components na a nnukwu sectional size na na., Mechanical Gears, Gear aro, isi axis, valvụ mkpanaka, Mechanical akụkụ - njikọ mkpanaka, bolt na nut, Multidiameter aro, Nrụgide arịa, enweghị nkebi anwụrụ