EN10025-6 S620QL1 daidai, EN10025-6 S620QL1 karfe farantin karfe, EN10025-6 S620QL1 karfe daidai, EN10025-6 S620QL1 sinadaran abun da ke ciki, EN10025-6 S620QL1
Quenched da tempered karfe farantin S620QL1 wanda yake a cikin EN 10025-6 fasahar bayarwa yanayi ga lebur kayayyakin na high yawan amfanin ƙasa ƙarfi tsarin steels a QT bayarwa yanayin.The karfe yin tsari na high ƙarfi karfe farantin S620QL1 za su kasance daidai da EN 10025-1 Idan an ƙayyade a lokacin oda za a ba da rahoton aikin yin ƙarfe ga mai siye.Ya kamata a yi gwajin tasirin ƙarancin zafin jiki don babban ƙarfin karfe S620QL1 a debe 60 centigrade.
Bukatun Fasaha & Ƙarin Sabis:
Gwajin tasirin ƙarancin zafin jiki
Quenching da Tempering zafi magani
Gwajin Ultrasonic karkashin EN 10160, ASTM A435, A577, A578
An ba da takardar shaidar gwaji ta Orginal Mill a ƙarƙashin EN 10204 FORMAT 3.1 /3.2
Shot fashewa da Fenti, Yanke da walda kamar yadda ƙarshen buƙatun mai amfani
TS EN 10025-6 S620QL1 quenched da zafin karfe farantin karfe
Daraja | C% | Si % | Mn % | P% | S% | N % | B% | Cr % |
Saukewa: S620QL1 | 0.200 | 0.800 | 1.700 | 0.020 | 0.010 | 0.015 | 0.005 | 1.500 |
Ku % | Mo % | Nb % | Ni % | Ti % | V % | Zr % | ||
0.500 | 0.700 | 0.060 | 2.000 | 0.050 | 0.120 | 0.150 |
TS EN 10025-6 S620QL1 kaddarorin inji
Daraja | Kauri (mm) | Min Haɓaka (Mpa) | Tensile (MPa) | Tsawaitawa (%) | Min Tasirin Makamashi | |
Saukewa: S620QL1 | 8mm-50mm | Min 620Mpa | 700-890Mpa | 15% | -60 | Min 30J |
51mm-100mm | Min 580Mpa | 700-890Mpa | 15% | -60 | Min 30J | |
101-150mm | Min 560Mpa | 650-830Mpa | 15% | -60 | Min 30J |
Idan kuna da wata buƙata a cikin EN10025-6 S620QL1 quenched da farantin karfe, da fatan za a iya tuntuɓar mu.