Alloy 321 (UNS S32100) titanium stabilized austenitic bakin karfe tare da mai kyau janar lalata juriya. Yana da kyakkyawan juriya ga lalatawar intergranular bayan bayyanar yanayin zafi a cikin kewayon hazo na chromium carbide na 800 – 1500°F (427 – 816°C). Alloy yana tsayayya da iskar shaka zuwa 1500°F (816°C) kuma yana da mafi girman ragi da kaddarorin karyewar damuwa fiye da alloys 304 da 304L. Hakanan yana da taurin ƙarancin zafin jiki mai kyau.
Alloy 321H (UNS S 32109) shine mafi girman nau'in carbon (0.04 - 0.10) na gami. An ƙirƙira shi don haɓaka juriya mai rarrafe kuma don ƙarin ƙarfi a yanayin zafi sama da 1000oF (537°C). A mafi yawan lokuta, abun cikin carbon na farantin yana ba da takaddun shaida biyu.
Alloy 321 ba za a iya taurare da zafi magani, kawai ta hanyar sanyi aiki. Ana iya walda shi cikin sauƙi da sarrafa shi ta daidaitattun ayyukan ƙirƙira kanti.
Aikace-aikace gama gari
Aerospace - piston injin manifolds
Gudanar da Sinadarai
Fadada haɗin gwiwa
Gudanar da Abinci - kayan aiki da ajiya
Gyaran Man Fetur - sabis na polythionic acid
Maganin Sharar gida - thermal oxidizers
Abubuwan Sinadarai:
% |
Cr |
Ni |
C |
Si |
Mn |
P |
S |
N |
Ti |
Fe |
321 |
min:17.0 |
min: 9.0 |
max:0.08 |
max:0.75 |
max:2.0 |
max:0.045 |
max:0.03 |
max:0.10 |
min: 5*(C+N) |
Ma'auni |
321H |
min:17.0 |
min: 9.0 |
min: 0.04 |
min:18.0 |
max:2.0 |
max:0.045 |
max:0.03 |
max:0.10 |
min: 5*(C+N) |
Ma'auni |
Kayayyakin Injini:
Daraja |
Ƙarfin Ƙarfi |
Ƙarfin Haɓaka 0.2% |
Tsawaitawa - |
Tauri |
321 |
75 |
30 |
40 |
217 |
Abubuwan Jiki:
Denstiy |
Coefficient na |
Fadada zafin zafi (min/a) -°F |
Thermal Conductivity BTU/hr-ft-°F |
Takamaiman Zafi BTU/lbm -°F |
Modules na Ƙarfafawa (annealed)2-psi |
ku 68°F |
da 68-212 ° F |
da 68-1832°F |
da 200 ° F |
da 32-212 ° F |
cikin tashin hankali (E) |
0.286 |
9.2 |
20.5 |
9.3 |
0.12 |
28 x106 |