Co-dhèanamh ceimigeach agus feartan meacanaigeach:
ASTM A537 Clas 3 (A537CL3)
Stuth |
c |
Mn |
Si |
≤ |
S≤ |
ASTM A537 Clas 3 (A537CL3) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
Stuth |
Neart tensile (MPa) |
Neart toraidh (MPa) MIN |
% Elongation MIN |
ASTM A537 Clas 3 (A537CL3) |
485-690 |
275-380 |
20 |
ASTM A537 Clas 2 (A537CL2)
Stuth |
c |
Mn |
Si |
≤ |
S≤ |
ASTM A537 Clas 2 (A537CL2) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
Stuth |
Neart tensile (MPa) |
Neart toraidh (MPa) MIN |
% Elongation MIN |
ASTM A537 Clas 2 (A537CL2) |
485-690 |
315-415 |
20 |
ASTM A537 Clas 1 (A537CL1)
Stuth |
c |
Mn |
Si |
≤ |
S≤ |
ASTM A537 Clas 1 (A537CL1) |
0.24 |
0.13-0.55 |
0.92-1.72 |
0.035 |
0.035 |
Stuth |
Neart tensile (MPa) |
Neart toraidh (MPa) MIN |
% Elongation MIN |
ASTM A537 Clas 1 (A537CL1) |
450-585 |
310 |
18 |
Sgrìobhainnean air an Iomradh
Inbhean ASTM:
A20 /A20M: Sònrachadh airson Riatanasan Coitcheann airson Plataichean Soithichean Brùthadh
A435 / A435: Airson Sgrùdadh Ultrasonach Beam Dìreach air Plate Stàilinn
A577 / A577M: Airson Sgrùdadh Ultrasonic Angle-Beam air lannan stàilinn
A578 / A578M: Airson Sgrùdadh Ultrasonach le giùlan dìreach air lannan stàilinn rolaichte airson tagraidhean sònraichte
Notaichean saothrachaidh:
Bidh plàta stàilinn fo ASTM A537 Clas 1, 2 agus 3 air a mharbhadh le stàilinn agus a rèir riatanas meud gràin austenitic grinn de Shònrachadh A20 / A20M.
Dòighean làimhseachaidh teas:
Bidh a h-uile truinnsear fo ASTM A537 air a làimhseachadh le teas mar a leanas:
Feumaidh truinnsearan ASTM A537 Clas 1 a bhith àbhaisteach.
Feumaidh truinnsearan Clas 2 agus Clas 3 a bhith air an cuartachadh agus air an teannachadh. Cha bhith an teòthachd measaidh airson truinnsearan Clas 2 nas ìsle na 1100 ° F [595 ° C] agus gun a bhith nas ìsle na 1150 ° F [620 ° C] airson truinnsearan Clas 3.