Gewicht % (alle wearden binne maksimaal, útsein as in berik oars oanjûn is)
Elemint | 347 | 347H |
Chromium | 17.00 min.-19.00 max. | 17.00 min.-19.00 max. |
Nikkel | 9.00 min.-13.00 max. | 9.00 min.-13.00 max. |
Koalstof | 0.08 | 0.04 min.-0.10 max. |
Mangaan | 2.00 | 2.00 |
Fosfor | 0.045 | 0.045 |
Sulphur | 0.03 | 0.03 |
Silisium | 0.75 | 0.75 |
Kolumbium en Tantaal | 10 x (C + N) min.-1.00 max. | 8 x (C + N) min.-1.00 max. |
Izer | Lykwicht | Lykwicht |
FYSIKE EIGENSKIPPEN
Tichte: 0,288 lbs/in3 7,97 g/cm3 Elektryske wjerstân: microhm-in (mikrohm-cm): 68 °F (20 °C): 28,7 (73)
Spesifike waarmte: BTU/lb/°F (kJ/kg•K):
32 - 212 °F (0 - 100 °C): 0,12 (0,50)
Thermyske konduktiviteit: BTU/hr/ft2/ft/°F (W/m•K):
By 212 °F (100 °C): 9,3 (16,0)
By 932 °F (500 °C): 12,8 (22,0)
Gemiddelde termyske útwreidingskoëffisjint: yn/in/°F (µm/m•K):
32 - 212 °F (0 - 100 °C): 9,3 x 10,6 (16,6)
32 - 1000 °F (0 - 538 °C): 10,5 x 10,6 (18,9)
32 - 1500 °F (0 - 873 °C): 11,4 x 10,6 (20,5)
Elasticiteitsmodulus: ksi (MPa):
28 x 103 (193 x 103) yn spanning
11 .2 x 103 (78 x 103) yn torsion
Magnetic Permeability: H = 200 Oersteds: Annealed < 1.02 max
Smeltberik: 2500 - 2550 °F (1371 - 1400 °C)