ASTM ASME (S)A-335/(S)A-335M Qualität und chemische Zusammensetzung
Grad |
UNS |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Mo |
P1 |
K11522 |
0.10~0.20 |
0.30~0.80 |
0.025 |
0.025 |
0.10~0.50 |
- |
0.44~0.65 |
P2 |
K11547 |
0.10~0.20 |
0.30~0.61 |
0.025 |
0.025 |
0.10~0.30 |
0.50~0.81 |
0.44~0.65 |
P5 |
K41545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
4.00~6.00 |
0.44~0.65 |
P5b |
K51545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.00~2.00 |
4.00~6.00 |
0.44~0.65 |
P5c |
K41245 |
0.12 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
4.00~6.00 |
0.44~0.65 |
P9 |
S50400 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50~1.00 |
8.00~10.00 |
0.44~0.65 |
P11 |
K11597 |
0.05~0.15 |
0.30~0.61 |
0.025 |
0.025 |
0.50~1.00 |
1.00~1.50 |
0.44~0.65 |
P12 |
K11562 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
0.80~1.25 |
0.44~0.65 |
P15 |
K11578 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.15~1.65 |
- |
0.44~0.65 |
P21 |
K31545 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
2.65~3.35 |
0.80~1.60 |
P22 |
K21590 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
1.90~2.60 |
0.87~1.13 |
P91 |
K91560 |
0.08~0.12 |
0.30~0.60 |
0.020 |
0.010 |
0.20~0.50 |
8.00~9.50 |
0.85~1.05 |
P92 |
K92460 |
0.07~0.13 |
0.30~0.60 |
0.020 |
0.010 |
0.50 |
8.50~9.50 |
0.30~0.60 |
Hinweis: (S)A335 P91 andere chemische Zusammensetzungen sind: V 0,18~0,25; N 0,030–0,070; Ni ≤ 0,40; Al ≤ 0,04 ; Anzahl: 0,06–0,10
(S)A335 P92 andere chemische Zusammensetzungen sind: V 0,15~0,25; N 0,030–0,070; Ni ≤ 0,40; Al ≤ 0,04 ; Nb 0,04–0,09; W 1,5–2,00; B 0,001~0,006
Mechanische Eigenschaften
Zugfestigkeit, MPa |
Streckgrenze, MPa |
Dehnung, % |
415 Min |
205 Min |
30 Minuten |
Außendurchmesser und Toleranz
ASTM A450 |
Warmgewalzt |
Außendurchmesser, mm |
Toleranz, mm |
OD≤101,6 |
+0.4/-0.8 |
101,6<OD≤190,5 |
+0.4/-1.2 |
190,5<OD≤228,6 |
+0.4/-1.6 |
Kaltgezogen |
Außendurchmesser, mm |
Toleranz, mm |
AD<25,4 |
±0,10 |
25,4 ≤ OD ≤ 38,1 |
±0,15 |
38,1<OD<50,8 |
±0,20 |
50,8 ≤ OD < 63,5 |
±0,25 |
63,5 ≤ OD < 76,2 |
±0,30 |
76,2 ≤ OD ≤ 101,6 |
±0,38 |
101,6<OD≤190,5 |
+0.38/-0.64 |
190,5<OD≤228,6 |
+0.38/-1.14 |
ASTM A530 und ASTM A335 |
NPS |
Außendurchmesser, Zoll |
Toleranz, mm |
1/8≤OD≤1-1/2 |
±0,40 |
1-1/2
±0,79 |
|
4<OD≤8 |
+1.59/-0.79 |
8<OD≤12 |
+2.38/-0.79 |
OD>12 |
±1 % |
Wandstärke und Toleranz
ASTM A450 |
Warmgewalzt |
Außendurchmesser, mm |
Toleranz, % |
OD≤101,6, WT≤2,4 |
+40/-0 |
OD≤101,6, 2,4<WT≤3,8 |
+35/-0 |
OD≤101,6, 3,8<WT≤4,6 |
+33/-0 |
OD≤101,6, WT>4,6 |
+28/-0 |
OD>101,6, 2,4<WT≤3,8 |
+35/-0 |
OD>101,6, 3,8<WT≤4,6 |
+33/-0 |
OD>101,6, WT>4,6 |
+28/-0 |
Kaltgezogen |
Außendurchmesser, mm |
Toleranz, % |
OD≤38,1 |
+20/-0 |
OD>38,1 |
+22/-0 |
ASTM A530 |
NPS |
Außendurchmesser, Zoll |
Toleranz, % |
1/8≤OD≤2-1/2 |
+20.0/-12.5 |
3≤OD≤18, WT/OD≤5% |
+22.5/-12.5 |
3≤OD≤18, WT/OD>5% |
+15.0/-12.5 |
OD≥20, WT/OD≤5% |
+22.5/-12.5 |
OD≥20, WT/OD>5% |
+15.0/-12.5 |
StandardASTM A335 – für nahtlose Rohre aus ferritischem legiertem Stahl für den Einsatz bei hohen Temperaturen
ASTM A519 – für nahtlose mechanische Rohre aus Kohlenstoff- und legiertem Stahl
ASTM A213 – für nahtlose ferritische und austenitische Kessel-, Überhitzer- und Wärmetauscherrohre aus legiertem Stahl