Dur Di-staen 347 / 347H BWSING
Dur Di-staen 347 / 347H TEE
Pwysau % (uchafswm yw pob gwerth oni nodir amrediad fel arall)
Elfen | 347 | 347H |
Cromiwm | 17.00 mun.-19.00 max. | 17.00 mun.-19.00 max. |
Nicel | 9.00 mun.-13.00 max. | 9.00 mun.-13.00 max. |
Carbon | 0.08 | 0.04 mun.-0.10 max. |
Manganîs | 2.00 | 2.00 |
Ffosfforws | 0.045 | 0.045 |
Sylffwr | 0.03 | 0.03 |
Silicon | 0.75 | 0.75 |
Columbium a Tantalum | 10 x (C + N) min.-1.00 max. | 8 x (C + N) min.-1.00 max. |
Haearn | Cydbwysedd | Cydbwysedd |
EIDDO CORFFOROL
Dwysedd: 0.288 lbs /in3 7.97 g /cm3 Gwrthedd Trydanol: microhm-in (microhm-cm): 68 °F (20 °C): 28.7 (73)
Gwres Penodol: BTU /lb/°F (kJ / kg•K):
32 - 212 °F (0 - 100 °C): 0.12 (0.50)
Dargludedd Thermol: BTU /hr/ft2/ft/°F (W /m•K):
Ar 212 °F (100 °C): 9.3 (16.0)
Ar 932 °F (500 °C): 12.8 (22.0)
Cyfernod Cymedr Ehangu Thermol: yn / mewn / °F (µm / m•K):
32 - 212 °F (0 - 100 °C): 9.3 x 10·6 (16.6)
32 - 1000 °F (0 - 538 °C): 10.5 x 10·6 (18.9)
32 - 1500 °F (0 - 873 °C): 11.4 x 10·6 (20.5)
Modwlws Elastigedd: ksi (MPa):
28 x 103 (193 x 103) mewn tensiwn
11 .2 x 103 (78 x 103) mewn dirdro
Athreiddedd Magnetig: H = 200 Oersteds: Annealed < 1.02 max
Amrediad Toddi: 2500 - 2550 °F (1371 - 1400 °C)