ASTM ASME (S)A-335/(S)A-335M Grade è Composizione Chimica
Grade |
UNS |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Mo |
P1 |
K11522 |
0.10~0.20 |
0.30~0.80 |
0.025 |
0.025 |
0.10~0.50 |
- |
0.44~0.65 |
P2 |
K11547 |
0.10~0.20 |
0.30~0.61 |
0.025 |
0.025 |
0.10~0.30 |
0.50~0.81 |
0.44~0.65 |
P5 |
K41545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
4.00~6.00 |
0.44~0.65 |
P5b |
K51545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.00~2.00 |
4.00~6.00 |
0.44~0.65 |
P5c |
K41245 |
0.12 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
4.00~6.00 |
0.44~0.65 |
P9 |
S50400 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50~1.00 |
8.00~10.00 |
0.44~0.65 |
P11 |
K11597 |
0.05~0.15 |
0.30~0.61 |
0.025 |
0.025 |
0.50~1.00 |
1.00~1.50 |
0.44~0.65 |
P12 |
K11562 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
0.80~1.25 |
0.44~0.65 |
P15 |
K11578 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.15~1.65 |
- |
0.44~0.65 |
P21 |
K31545 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
2.65~3.35 |
0.80~1.60 |
P22 |
K21590 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50 |
1.90~2.60 |
0.87~1.13 |
P91 |
K91560 |
0.08~0.12 |
0.30~0.60 |
0.020 |
0.010 |
0.20~0.50 |
8.00~9.50 |
0.85~1.05 |
P92 |
K92460 |
0.07~0.13 |
0.30~0.60 |
0.020 |
0.010 |
0.50 |
8.50~9.50 |
0.30~0.60 |
Nota: (S) A335 P91 altre cumpusizioni chimichi sò: V 0,18 ~ 0,25; N 0,030 ~ 0,070; Ni ≤ 0,40; Al ≤ 0,04; Nb 0,06 ~ 0,10
(S) A335 P92 altri cumpusizioni chimichi sò: V 0,15 ~ 0,25; N 0,030 ~ 0,070; Ni ≤ 0,40; Al ≤ 0,04; Nb 0,04 ~ 0,09; W 1,5 ~ 2,00; B 0,001 ~ 0,006
Pruprietà meccanica
Resistance à la traction, MPa |
Rendimentu, MPa |
allungamentu, % |
415 min |
205 min |
30 min |
Diametru Esternu è Tolleranza
ASTM A450 |
Laminatu à caldu |
Diametru fora, mm |
Tolleranza, mm |
OD≤101,6 |
+0.4/-0.8 |
101,6<OD≤190,5 |
+0.4/-1.2 |
190,5<OD≤228,6 |
+0.4/-1.6 |
Cold Drawn |
Diametru fora, mm |
Tolleranza, mm |
OD<25.4 |
± 0,10 |
25,4≤OD≤38,1 |
± 0,15 |
38.1<OD<50.8 |
± 0,20 |
50,8≤OD<63,5 |
± 0,25 |
63,5≤OD<76,2 |
± 0,30 |
76,2≤OD≤101,6 |
± 0,38 |
101,6<OD≤190,5 |
+0.38/-0.64 |
190,5<OD≤228,6 |
+0.38/-1.14 |
ASTM A530 è ASTM A335 |
NPS |
Diametru esternu, inch |
Tolleranza, mm |
1/8≤OD≤1-1/2 |
± 0,40 |
1-1/2<OD≤4 |
± 0,79 |
4<OD≤8 |
+1.59/-0.79 |
8<OD≤12 |
+2.38/-0.79 |
OD> 12 |
± 1% |
Spessore di u muru è Tolleranza
ASTM A450 |
Laminatu à caldu |
Diametru fora, mm |
Tolleranza, % |
OD≤101.6, WT≤2.4 |
+40/-0 |
OD≤101.6, 2.4<WT≤3.8 |
+35/-0 |
OD≤101.6, 3.8<WT≤4.6 |
+33/-0 |
OD≤101.6, WT> 4.6 |
+28/-0 |
OD>101.6, 2.4<WT≤3.8 |
+35/-0 |
OD>101.6, 3.8<WT≤4.6 |
+33/-0 |
OD> 101,6, WT> 4,6 |
+28/-0 |
Cold Drawn |
Diametru fora, mm |
Tolleranza, % |
OD≤38,1 |
+20/-0 |
OD> 38,1 |
+22/-0 |
ASTM A530 |
NPS |
Diametru esternu, inch |
Tolleranza, % |
1/8≤OD≤2-1/2 |
+20.0/-12.5 |
3≤OD≤18, WT/OD≤5% |
+22.5/-12.5 |
3≤OD≤18, WT/OD>5% |
+15.0/-12.5 |
OD≥20, WT/OD≤5% |
+22.5/-12.5 |
OD≥20, WT/OD>5% |
+15.0/-12.5 |
StandardASTM A335--per Tubi d'acciaio in lega ferriticu senza saldatura per serviziu à alta temperatura
ASTM A519--per Tubi Meccanici di Carbone è Alloy Steel senza saldatura
ASTM A213--per i tubi senza saldatura per caldaie, surriscaldatori e scambiatori di calore in acciaio in lega ferritica è austenitica