Mga produkto
We have professional sales team numbered 200 with more than 16 years experience.
Posisyon:
Balay > Mga produkto > Steel Plate > Steel Plate sa Pagbuhat sa mga Barko
CCS Shipbuilding steel plate
CCS Shipbuilding Plate
CCS Shipbuilding Plate
CCS Shipbuilding Plate

CCS nga paghimo sa barko nga steel plate

CCS shipbuilding plate grade AQ DQ EQ FQ AH EH FH 36 40 47 51 63 70 kemikal ug mekanikal nga mga kabtangan
Pagpaila sa produkto
CCS Shipbuilding Plate

CCS Grade FQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
690 770-940 14

CCS Grade EQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
690 770-940 14

CCS Grade DQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.035 0.035 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
690 770-940 14--16

CCS Grade AQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
690 770-940 14

CCS Grade EQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
620 720-890 15

CCS Grade FQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
620 720-890 15

CCS Grade AQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
620 720-890 15

CCS Grade EQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
550 670-830 16

CCS Grade FQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
550 670-830 16

CCS Grade AQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.60 0.030 0.030 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
550 670-830 16

CCS Grade EQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
500 610-770 16

CCS Grade FQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
500 610-770 16

CCS Grade AQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
500 610-770 16

CCS Grade EQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
460 570-720 17

CCS Grade FQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
460 570-720 17

CCS Grade AQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
460 570-720 17
Teknikal nga datos

CCS Grade EH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
390 510-660 20

CCS Grade FH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.16 0.50 0.90-1.60 0.020 0.020 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.80 0.08 0.009
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
390 510-660 20

CCS Grade AH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.030 0.030 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
390 510-660 20

CCS Grade EH36 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Kalig-on sa ani (MPa) min. Kusog sa Tensile (MPa) Elongation min. %
355 490-630 21

CCS/E Normal nga Kusog Max nga Komposisyon sa Kemikal sa Hot-rolled

elemento CCS E Max % elemento CCS E Max %
C 0.21 Ni
Mn 0.60 Mo
Si 0.1-0.35 Si Al
S 0.035 Nb
P 0.035 V
Cu Ti
Ang Cr N
Pagkasensitibo sa Crack: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas sa Carbon: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
CCS/E Normal nga kusog nga kabtangan sa Hot-rolled
Grado Gibag-on Kalig-on sa ani Kusog sa Tensile Elongation Epekto nga Enerhiya
(mm) MPa (min) MPa % (min) (KV J) (min)
-20 degree
CCS E 8-240 235 400-520 22 27J

Mubo nga sulat: ang epekto sa enerhiya ubos sa dili kaayo 50mm gibag-on; longhitudinal min epekto enerhiya

CCS/D Normal Strength Max Chemical Composition sa Hot-rolled

elemento CCS D  Max % elemento CCS D  Max %
C 0.21 Ni
Mn 0.60 Mo
Si 0.1-0.35 Si Al
S 0.035 Nb
P 0.035 V
Cu Ti
Ang Cr N
Pagkasensitibo sa Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas sa Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/D Normal nga kusog nga kabtangan sa Hot-rolled

Grado Gibag-on Kalig-on sa ani Kusog sa Tensile Elongation Epekto nga Enerhiya
(mm) MPa (min) MPa % (min) (KV J) (min)
-20 degree
CCS D 8-240 235 400-520 22 27J

Mubo nga sulat: ang epekto sa enerhiya ubos sa dili kaayo 50mm gibag-on; longhitudinal min epekto enerhiya

CCS/B Normal Strength Max Chemical Composition sa Hot-rolled

elemento CCS B  Max % elemento CCS B  Max %
C 0.21 Ni
Mn 0.80 Mo
Si 0.35 Si Al
S 0.035 Nb
P 0.035 V
Cu Ti
Ang Cr N
Pagkasensitibo sa Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas sa Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/B Normal nga kusog nga kabtangan sa Hot-rolled

Grado Gibag-on Kalig-on sa ani Kusog sa Tensile Elongation Epekto nga Enerhiya
(mm) MPa (min) MPa % (min) (KV J) (min)
0 degree
CCS B 8-240 235 400-520 22 27J

Mubo nga sulat: ang epekto sa enerhiya ubos sa dili kaayo 50mm gibag-on; longhitudinal min epekto enerhiya

CCS/Usa ka Normal Strength Max Chemical Composition sa Hot-rolled

elemento CCS A Max % elemento CCS A Max %
C 0.21 Ni
Mn 2.5*C MIN Mo
Si 0.50 Si Al
S 0.035 Nb
P 0.035 V
Cu Ti
Ang Cr N

Pagkasensitibo sa Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas sa Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/Usa ka Normal nga kusog nga kabtangan sa Hot-rolled

Grado Gibag-on Kalig-on sa ani Kusog sa Tensile Elongation Epekto nga Enerhiya
(mm) MPa (min) MPa % (min) (KV J) (min)
20 degree
CCS A 8-240 235 400-520 22
Mubo nga sulat: ang epekto sa enerhiya ubos sa dili kaayo 50mm gibag-on; longhitudinal min epekto enerhiya